环氧地坪色差和环氧地坪失光现象的原因解决方案

作者:地坪 来源:未知 日期:2017-8-26 14:14:39 人气: 标签:
导读:环氧树脂地坪漆中的溶剂大多是对人体是有害的,环氧树脂地坪漆本身无毒,但环氧树脂地坪漆固化剂有毒,如MDA、TDl是致癌物质,最要命的是MDA、TDl这些致癌物质会

环氧树脂地坪漆中的溶剂大多是对人体是有害的,环氧树脂地坪漆本身无毒,但环氧树脂地坪漆固化剂有毒,如MDATDl是致癌物质,最要命的是MDATDl这些致癌物质会残留在环氧树脂地坪内,慢慢挥发出来。这就是美国人不做环氧树脂地坪的根本原因,所以环氧树脂地坪漆也不适合做家装。

 Solvent in epoxy floor paint is mostly is harmful to human body, non-toxic, epoxy floor paint itself but toxic epoxy floor paint curing agent, such as MDA, TDl is carcinogenic substance, is the most terrible of MDA, TDl these carcinogens can residues in epoxy floor paint, slowly evaporates. This is the fundamental reason why americans do not make epoxy resins, so the epoxy resin floor paint is not suitable for home decoration.

20175月,北京市高调宣布,明确将环氧地坪涂料列入调整退出的重点行业,首都的标本作用,将成为其他大城市学习的榜样。代之而起的是做纳路特混凝土密封固化剂抛光混凝土地坪。纳路特科技研发的金钻磨石等系列抛光混凝土产品是装修装饰行业替代环氧的最佳选择。纳路特是地面终极解决方案,产品无(无TVOC、无毒、无缝),防(防尘、防滑、防水)、抗(抗压、抗渗、抗老化)、耐(耐腐蚀、耐摩擦、耐刮伤),规格高端,样式多选。签约入选中央电视台国家品牌计划。

In May 2017, Beijing announced a high-profile decision to include epoxy floor coatings as a key industry for the adjustment and withdrawal of the capital, which will serve as an example for other big cities to learn from. Instead, it was made of the concrete and concrete floor of the nalu concrete sealant. A series of polished concrete products, such as gold diamond grindstone, developed by nalot technology, are the best alternative to epoxy in decoration industry. Path is to ground the ultimate solution, the product without no TVOC, non-toxic, seamless (), proof, dustproof, non-slip, waterproof), fight (compressive strength, permeability resistance, anti-aging), resistance, corrosion resistance, resistance to friction, scratch), specifications, high-end style multi-select. Signed up for the national brand plan of CCTV.

一、出现环氧地坪色差的原因分析和预防处理

 I. analysis and prevention of the color difference of epoxy floors

环氧地坪的施工团队经常会遇到自己完成的项目颜色与目标颜色有些差别,这种情况一般在验收过程中会受到客户的质疑,那么是什么情况导致得环氧地坪颜色不纯呢?又有哪些方法可以预防这种情况发生?

Epoxy floor construction team often they completed project some of difference colorwith the target color, this kind of situation usually will be questioned by the customer in the process of acceptance, then what is the result of epoxy floor paint color is not pure? What other methods can prevent this from happening?

1、环氧地坪施工期间,在底层涂膜没有完全干的情况下继续施工,容易导致颜色混合一起引起渗色;

1. During the construction period of epoxy floor, continuous construction is carried out under the condition that the underlying coating is not completely dry, which can lead to color mixing.

2、环氧地坪面漆中含有溶解能力很强的溶剂,例如酯类、酮类等;

 2. Epoxy floor paint contains solvents, such as ester and ketones, which are highly solvent.

3、环氧地坪底漆与面漆溶剂调配问题;

3. Preparation of epoxy floor primer and surface paint solvent; 

4、颜色深浅搭配问题;

 4. Color depth matching problem;

5、底漆最好选用无机颜料,应避免底漆中混入沥青和杂酚油等。

It is best to choose inorganic pigments for the primer and avoid the mixture of asphalt and creosote in the primer. 

地坪渗色是从表面上看地坪颜色不一的现象,渗色是因为环氧地坪面涂覆盖在另一种颜色的环氧地坪底涂时,底涂部分颜色渗入面涂颜色中导致面层涂膜颜色变色的问题。

 Floor bleeding from the phenomenon of surface ground color differ, bleeding because epoxy floor surface coated cover at the end of another kind of color epoxy floor coating, bottom color part into color color resulting in surface coating surface discoloration.

二、出现环氧地坪失光的原因分析和预防处理

 Ii. The cause analysis and prevention of the loss of the epoxy floor

众所周知,环氧地坪的主要成分是环氧树脂,在施工过程中,添加剂的使用正确与否以及环境因素等,都会对环氧树脂的特性产生一定的影响,所以经常会遇到验收环氧地坪的时候发现产品失去光泽,那么我们在施工环氧地坪的时候如何才能保证环氧地坪不会失去光泽呢?

 As is known to all, the main components of the epoxy floor is epoxy resin, in the process of construction, the use of additives is correct or not, and environmental factors, etc., will be a certain influence on the properties of epoxy resin, so often the epoxy floor level to find acceptance product lose luster, so when we are in the construction of epoxy floor how can ensure epoxy floor will not lose its luster?

1、施工场所湿度太大(相对湿度超过85%),挥发性漆的涂膜轻易吸收水分而发白发光。预防:施工场所的湿度不宜过大。

 1. The humidity in the construction site is too large (relative humidity is over 85%), the film of volatile paint absorbs moisture easily and hair white. Prevention: the humidity in the construction site should not be excessive.

2、环氧地坪施工中稀释剂用量过多或加入了煤油一类的高沸点稀释剂。预防:稀释剂用量不宜过多,应避免煤油一类的高沸点溶剂的加入。

 2. Excessive amount of diluent in epoxy floor construction or high boiling point thinner such as kerosene. Prevention: the amount of diluent should not be too much, should avoid the high boiling point solvent such as kerosene.

3、环氧地坪物面处理不干净,含有酸、碱、油污、蜡质和水分等。这就要求我们施工前,被涂物表面应充分处理干净。

3. Epoxy ground surface treatment is not clean, including acid, alkali, oil pollution, wax and water. This requires that the coated surfaces should be fully cleaned before construction. 

4、漆中颜料的水分含量过高或施工中混入水分。预防:环氧地坪应控制颜料的含水量,施工中避免混入水分。

4. Excessive water content of pigment in paint or water in construction. Prevention: epoxy floor should control the moisture content of paint, and avoid mixing water in construction. 

5、被涂物表面过分粗拙或多孔,未涂封锁底漆会发生环氧地坪失光现象。此种原因引起的环氧地坪漆失光就需要我们物面应用底漆封锁,腻子填平,打磨。

 5. Overrough or porous on the surface of the coated surface, and the loss of light in epoxy floor will occur without the sealing primer. This kind of reason causes epoxy floor paint to be out of light and needs to be used to apply the primer seal, putty filling, polishing.

6、涂膜未完全干透之前遇雨水或露水。预防:涂膜在干燥过程中要防止雨水或露水浸润。

6. Rain or dew before the coating is completely dry. Prevention: to prevent rain or dew infiltration during drying.

7、涂膜软,耐划伤机能不好。预防:按被涂物的使用前提,选用耐候性、抗划伤机能良好的涂料。

7. The film is soft and can not function well. Prevention: according to the precondition of being painted, the coatings with good weatherability and anti-scratch function are selected.